Light weight aggregate and process of making it |
|||||||
申请号 | US22860862 | 申请日 | 1962-10-05 | 公开(公告)号 | US3215542A | 公开(公告)日 | 1965-11-02 |
申请人 | TINKER CHARLES D; | 发明人 | TINKER CHARLES D; | ||||
摘要 | |||||||
权利要求 | 1. A PROCESS OF FORMING A CERAMIC WHICH CONSISTS OF (1) SINTERING EXPANDED BLAST FURNACE SLAG AGGREGATE BY BRINGING IT TO A TEMPERATURE OF ABOUT 2000*F. DURING A PERIOD OF ABOUT SIX HOURS; (2) MIXING THE SINTERED EXPANDED BLAST FURNACE SLAG AGGREGATE WITH CLAY; (3) FORMING THE MIXTURE OF SLAG AND CLAY IN THE DESIRED FORM; AND FIRING THE FORMED MIXTURE OF SLAG AND CLAY AT A TEMPERATURE OF ABOUT 2000*F. 2. A PROCESS OF FORMING A STABILIZED EXPANDED SLAG AGGREGATE WHICH COMPRISES SINTERING THE EXPANDED SLAG AGGREGATE BY BRINGING IT TO A TEMPERATURE OF ABOUT 2000*F. DURING A PERIOD OF ABOUT SIX HOURS. |
||||||
说明书全文 |