Method for extrusion coating electric wires with a foamed polyolefin resin involving reduced die-plateout

阅读:634发布:2022-09-10

专利汇可以提供Method for extrusion coating electric wires with a foamed polyolefin resin involving reduced die-plateout专利检索,专利查询,专利分析的服务。并且A method for manufacturing electric wires insulated with a foamed polyolefin-series resin by continuous, stable extrusion wherein a foamable polyolefin-series resin composition prepared by mixing a polyolefin-series resin with a foaming agent comprising azodicarbonamide and at least 10 per cent by weight of a material having a solubility parameter of 12.0 or more based on the amount of said azodicarbonamide is used for insulation of electric conductor.,下面是Method for extrusion coating electric wires with a foamed polyolefin resin involving reduced die-plateout专利的具体信息内容。

1. A METHOD FOR MANUFACTURING ELECTRIC WIRES INSULATED WITH A FOAM POLYOLEFIN RESIN BY CONTINUOUS, STALE EXTRUSION WHEREIN A FOAMAABLE POLYOLEFIN RESIN COMPOSITION IS PREPARED BY MIXING A POLYOLEFIN RESIN WITH A FOAMING AGENT COMPRISING AZODICARBONAMIDE AND BETWEN ABOUT 10 AND 150 PERCENT BY WEIGHT OF AT LEAST ONE MATERIAL HAVING A SOLUBILITY PARAMETER OF AT LEAST 12.0 BASED ON THE AMOUNT OF SAID AZODICARBONAMIDE AND EXTRUDING IT ON AN ELECTRIC CONDUCTOR UNDER CONDITIONS IN WHICH SAID AZODICARBONAMIDE DECOMPOSES, SAID MATERIAL HAVING SAID SOLUBILITY PARAMETER BEING SELECTED FROM THE GROUP CONSISTING OF POLYHYDRIC ALCOHOLS HAVING LESS THAN EIGHT CARBON AOMS, ETHANOL AMINES HAVING LESS THAN SIX CARBON ATOMS, ALKANOLS HAVING LESS THAN THREE CARBON AOMS, DIMETHYL SULFOXIDE, CARBOXYMETHYL CELLULOSE, METHYL CELLULOSE, LIGNIN, LIGNIN SULFONIC ACID, LACTONES, ALKYL ACETAMIDES, ALKYLFORMAMIDES, PHENOLS, ETHYLENE CARBONATE, THIOUREA, SUCCINIMIDE, AND COMPOUNDS CONTAINING A 1,3,5-TRIAZINE RING EXPRESSED BY THE GENERAL FORMULA
2. A method according to claim 1 wherein the foamable polyolefin-series resin composition is extruded on an electric conductor in a thickness of less than 1.0 mm.
3. A method according to claim 1 wherein 10 to 150 per cent by weight of the material having a solubility parameter of 12.0 or more is added based on the amount of azodicarbonamide used.
4. A method according to claim 1 wherein the polyolefin-series resin is a homopolymer of olefins.
5. A method according to claim 1 wherein the polyolefin-series resin is a copolymer of olefins and vinyl monomers.
6. A method according to claim 1 wherein the polyolefin-series resin is polyethylene.
7. A method according to claim 1 wherein the polyolefin-series resin is polypropylene.
8. A method according to claim 1 wherein the foaming agent consists of azodicarbonamide alone.
9. A method according to claim 1 wherein the foaming agent consists of azodicarbonamide and another foaming agent thermally decomposable at the extrusion temperature of the foamable polyolefin-series resin composition.
10. A method according to claim 1 wherein the foaming agent consists of azodicarbonamide and a volatile liquid foaming agent that turns into gas at the extrusion temperature of the foamable polyolefin-series resin composition.
11. A method according to claim 1 wherein the foaming agent consists of azodicarbonamide and at least one gas.
12. A method according to claim 9 wherein the thermally decomposable foaming agent is at least one selected from the group consisting of p,p''-oxybisbenzenesulfonyl hydrazide, p-toluenesulfonyl semicarbazide, and dinitrosopentamethylene tetramine.
13. A method according to claim 10 wherein the volatile liquid foaming agent is at least one selected from the group consisting of benzene, hexane, isopentane, n-pentane, petroleum ether and monofluorotrichloromethane.
14. A method according to clam 11 wherein the gas used As a foaming agent is at least one selected from the group consisting of carbon dioxide gas, nitrogen gas, propane, butane and dichlorodifluoromethane.
15. A method according to claim 1 wherein the material having a solubility parameter of 12.0 or more is at least one selected from the group consisting of sodium salt of carboxymethyl cellulose, lignin, and melamine.
16. A method according to claim 1 wherein the material having a solubility parameter of 12.0 or more is at least one selected from the group consisting of ethylene glycol, glycerin and triethanolamine.
说明书全文
高效检索全球专利

专利汇是专利免费检索,专利查询,专利分析-国家发明专利查询检索分析平台,是提供专利分析,专利查询,专利检索等数据服务功能的知识产权数据服务商。

我们的产品包含105个国家的1.26亿组数据,免费查、免费专利分析。

申请试用

分析报告

专利汇分析报告产品可以对行业情报数据进行梳理分析,涉及维度包括行业专利基本状况分析、地域分析、技术分析、发明人分析、申请人分析、专利权人分析、失效分析、核心专利分析、法律分析、研发重点分析、企业专利处境分析、技术处境分析、专利寿命分析、企业定位分析、引证分析等超过60个分析角度,系统通过AI智能系统对图表进行解读,只需1分钟,一键生成行业专利分析报告。

申请试用

QQ群二维码
意见反馈