专利汇可以提供Structural element and a method for making such elements专利检索,专利查询,专利分析的服务。并且The invention relates to the providing of a novel structural element made by hydrothermal hardening of mixtures of siliceous material, lime or cement as binding agent, water and a solidifying or addition agent consisting of barium carbonate to form a compound of barium sulfate with water-soluble sulfates which be included as impurities within said siliceous material.,下面是Structural element and a method for making such elements专利的具体信息内容。

1. IN A METHOD OF MAKING STRUCTURAL ELEMENTS BY HARDENING A MIXTURE OF FILLING MATERIAL, A BINDING AGENT, AND WATER WHEREIN THE HARDENING IS CARRIED OUT IN A CONVENTIONAL MANNER IN AN AUTOCLAVE BY STEAM UNDER PRESSURE IN AXCESS OF ATMOSPHERIC PRESSURE AND AT A TEMPERATURE ABOVE 100*C, THE ADDITION OF AT LEAST ONE SOLIDIFYING AUXILIARY AGENT TO THE MIXTURE IN THE FORM OF CHEMICALLY GENERATED CORBONATE-PRODUCTS WHICH ARE INSOLUBLE OR DIFFICULTY SOLUBLE IN WATER AND WHICH AT LEAST INCLUDES BARIUM CARBONATE, THE IMPROVEMENT OF FREEZERPROOFNESS AND HIGH WET COMPRESSIVE STRENGHT COMPRISING THE ADDITION OF SAID BARIUM CARBONATE IN AN AMOUNT NECESSARY FOR CONVERSION OF ALL WATER-SOLUBLE SLFATES OF THE MIXTURE INTO WATER INSLOUBLE SULFATES, WHEREIN THE STOICHIOMETRIC EXCESS OF BARIUM CARBONATE IS 0.5 TO 2.0 PERCENT BY WEIGHT OF THE DRY FILLING MATERIAL AND AT LEAST IS 10 PERCENT THE WEIGHT OF THE AVERAGE OF WATER SOLUBLE SULFATES INCLUDED IN SAID MIXTURE.
2. A method in accordance with claim 1 wherein sAid stoichiometric excess of barium carbonate is substantially 1.25 percent by weight of the dry filling material and substantially 2.5 times the weight of the average of water soluble sulfates included in said mixture.
3. A method in accordance with claim 1 wherein the amount of barium carbonate is at least 1.5 percent by weight of the dry filling material.
4. A method in accordance with claim 1 wherein said chemically generated carbonate-products include calcium carbonate in an amount that is more than 1.0 percent by weight of the dry filling material.
5. A method in accordance with claim 4 wherein the amount of said calcium carbonate is 3.0 to 5.0 percent by weight of the dry filling material.
6. A method in accordance with claim 1 wherein the chemically generated carbonate added includes at least calcium carbonate in an amount greater than 1.0 percent by weight of the total dry filling material in addition to the stoichiometric amount of barium carbonate.
7. A method in accordance with claim 6 wherein the calcium carbonate added is in an amount that is 3.0 to 5.0 percent by weight of the total dry filling material in addition to the stoichiometric amount of barium carbonate.
8. A method in accordance with claim 1 wherein said filling material is siliceous sands from natural sources.
9. A method in accordance with claim 8 wherein said siliceous materials are substantially free from water soluble sulfates.
10. A method in accordance with claim 1 wherein the auxiliary agent consists of naturally occurring carbonate material.
11. A method in accordance with claim 10 wherein the auxiliary agent includes natural calcium carbonate raw materials.
12. A method in accordance with claim 10 wherein the auxiliary agent includes natural calcium-carbonate/magnesium-carbonate raw materials.
说明书全文
高效检索全球专利

专利汇是专利免费检索,专利查询,专利分析-国家发明专利查询检索分析平台,是提供专利分析,专利查询,专利检索等数据服务功能的知识产权数据服务商。

我们的产品包含105个国家的1.26亿组数据,免费查、免费专利分析。

申请试用

分析报告

专利汇分析报告产品可以对行业情报数据进行梳理分析,涉及维度包括行业专利基本状况分析、地域分析、技术分析、发明人分析、申请人分析、专利权人分析、失效分析、核心专利分析、法律分析、研发重点分析、企业专利处境分析、技术处境分析、专利寿命分析、企业定位分析、引证分析等超过60个分析角度,系统通过AI智能系统对图表进行解读,只需1分钟,一键生成行业专利分析报告。

申请试用

QQ群二维码
意见反馈