首页 / 专利库 / 建筑材料 / 粘合剂 / 水硬性胶凝材料 / 水泥 / 水泥添加剂 / Additive cement compositions and method

Additive cement compositions and method

阅读:541发布:2023-05-10

专利汇可以提供Additive cement compositions and method专利检索,专利查询,专利分析的服务。并且An additive composition for enhancing the properties of hydraulic cement compositions, and a hydraulic cement composition of enhanced properties, particularly useful in the cementing of wells, and methods of cementing geologic formations traversed by well bores are disclosed. The additive composition comprises a water soluble lignosulfonate or lignosulfonic acid or mixtures thereof, and tartaric acid or a salt of tartaric acid or mixtures thereof, and preferably about 3 parts calcium lignosulfonate and 1 part tartaric acid, although good results are obtained with 1 to 19 parts lignosulfonate or lignosulfonic acid and 19 to 1 parts tartaric acid or a salt of tartaric acid. The hydraulic composition includes a hydraulic cement and preferably about 11/2 % of the additive composition based on the weight of the cement; although , good results are obtained with from about 0.10% to about 3%, or higher, for example, for long life slurries. Especially good results are obtained when the hydraulic cement has been pretreated and aged as in our co-pending application filed Jan. 25, 1971, Ser. No. 109,606. The hydraulic cement composition has good viscosity and strength, ideal thickening times, and a reduced amount of mix water may be used thereby increasing the weight of the cement slurry. The method of performing cementing operations in geologic formations comprises introducing a slurry of the hydraulic cement composition in a well, positioning the cement slurry at cementing depth for bonding and plugging purposes, and allowing the cement slurry to harden. A number of examples are set forth disclosing the additive and hydraulic cement compositions, methods of making and using them.,下面是Additive cement compositions and method专利的具体信息内容。

  • 2. The hydraulic cement composition of claim 1 where the lignosulfonate is calcium lignosulfonate, and the selected member is tartaric acid.
  • 3. The hydraulic cement composition of claim 1 where the retarder composition consists essentially of about 3 parts calcium lignosulfonate and about 1 part tartaric acid.
  • 4. A hydraulic cement composition consisting of a substantially dry hydraulic cement free of substantial lumping intimately mixed with a small amount of liquid water and aged for a period of at least about 30 minutes, and about 0.10% to at least about 3.00% of a retarder composition based on the weight of the dry cement consisting essentially of from about 1 part to about 19 parts by weight of a member selected from the group consisting of a water soluble lignosulfonate, lignosulfonic acid and mixtures thereof, and from about 1 part to about 19 parts by weight of a member selected from the group consisting of tartaric acid, a salt of tartaric acid and mixtures thereof.
  • 5. The hydraulic cement composition of claim 4 where the lignosulfonate is calcium lignosulfonate, and the selected member is tartaric acid.
  • 6. The hydraulic cement composition of claim 4 where the retarder composition consists essentially of about 3 parts calcium lignosulfonate and about 1 part tArtaric acid.
  • 7. A hydraulic cement slurry including, the hydraulic cement composition of claim 1, the retarder composition being present in an amount effective to provide a thickening time of the order of at least about 3 hours at cementing depth.
  • 8. The hydraulic cement slurry of claim 7 where the lignosulfonate is calcium lignosulfonate, and where the selected member is tartaric acid.
  • 9. The hydraulic cement slurry of claim 7 where the retarder composition consists essentially of about 3 parts calcium lignosulfonate, and about 1 part tartaric acid.
  • 10. A hydraulic cement slurry including, a hydraulic cement prepared by intimately mixing the hydraulic cement with a small amount of liquid water and aging for a period of at least about 30 minutes before slurrying, and a retarder composition consisting essentially of from about 1 part to about 19 parts by weight of a member selected from the group consisting of a water soluble lignosulfonate, lignosulfonic acid and mixtures thereof, and from about 1 part to about 19 parts by weight of a member selected from the group consisting of tartaric acid, a salt of tartaric acid and mixtures thereof, the retarder composition being present in an amount effective to provide a thickening time of the order of at least about 3 hours at cementing depth.
  • 11. The hydraulic cement slurry of claim 10 where the lignosulfonate is calcium lignosulfonate, and where the selected member is tartaric acid.
  • 12. The hydraulic cement slurry of claim 10 where the retarder composition consists essentially of about 3 parts calcium lignosulfonate, and about 1 part tartaric acid.
  • 说明书全文
    高效检索全球专利

    专利汇是专利免费检索,专利查询,专利分析-国家发明专利查询检索分析平台,是提供专利分析,专利查询,专利检索等数据服务功能的知识产权数据服务商。

    我们的产品包含105个国家的1.26亿组数据,免费查、免费专利分析。

    申请试用

    分析报告

    专利汇分析报告产品可以对行业情报数据进行梳理分析,涉及维度包括行业专利基本状况分析、地域分析、技术分析、发明人分析、申请人分析、专利权人分析、失效分析、核心专利分析、法律分析、研发重点分析、企业专利处境分析、技术处境分析、专利寿命分析、企业定位分析、引证分析等超过60个分析角度,系统通过AI智能系统对图表进行解读,只需1分钟,一键生成行业专利分析报告。

    申请试用

    QQ群二维码
    意见反馈