专利汇可以提供Poling process for linear piezoelectric strain transducers专利检索,专利查询,专利分析的服务。并且A process for producing sufficient piezoelectric effect in plastic dielectric coaxial cable to obtain a highly sensitive linear strain transducer. The process combines a selected soak temperature profile with the application of high voltage DC to maximize sensitivity and uniformity. The plastic dielectric material exhibits a high level of piezoelectric activity when processed according to the invention so that, for example, the cable is sensitive to the passage of humans or vehicles when buried in the ground.,下面是Poling process for linear piezoelectric strain transducers专利的具体信息内容。

1. A method of poling manufactured coaxial cable having a plastic dielectric material disposed intermediate the inner conductor and the outer shield conductor of the cable to produce a linear piezoelectric transducer comprising the steps of: padding the barrel portion of a poling drum; loosely winding a length of the manufactured coaxial cable around said padded barrel portion of said drum; dressing the outer end of said cable to obtain a minimum of a 1 inch air gap between tHe inner conductor and the outer shield conductor of said cable; placing said drum holding said cable in a temperature chamber; connecting a source of high voltage to the dressed end of said cable between the inner conductor and the outer shield conductor of said cable; heating said chamber and said cable to an elevated temperature; cooling said chamber and said cable; disconnecting said source of high voltage; and aging said cable to overcome its high initial piezoelectric sensitivity which decays exponentially.
2. The method of claim 1 wherein: said source of high voltage has a potential of substantially 10, 000 volts DC.
3. The method of claim 1 wherein: said cable has a polyethylene dielectric, and said chamber is heated to a temperature in excess of 180* F.
4. The method of claim 3 wherein: said chamber is heated to substantially 200* F.
5. The method of claim 3 wherein: said chamber is held at said elevated temperature for substantially 7 hours.
6. The method of claim 5 wherein: said chamber is cooled to room temperature over a period of substantially 16 hours.
7. The method of claim 5 wherein: said chamber is cooled at an initial rate not in excess of 5* F per hour.
说明书全文
高效检索全球专利

专利汇是专利免费检索,专利查询,专利分析-国家发明专利查询检索分析平台,是提供专利分析,专利查询,专利检索等数据服务功能的知识产权数据服务商。

我们的产品包含105个国家的1.26亿组数据,免费查、免费专利分析。

申请试用

分析报告

专利汇分析报告产品可以对行业情报数据进行梳理分析,涉及维度包括行业专利基本状况分析、地域分析、技术分析、发明人分析、申请人分析、专利权人分析、失效分析、核心专利分析、法律分析、研发重点分析、企业专利处境分析、技术处境分析、专利寿命分析、企业定位分析、引证分析等超过60个分析角度,系统通过AI智能系统对图表进行解读,只需1分钟,一键生成行业专利分析报告。

申请试用

QQ群二维码
意见反馈